Isabelle Gensburger
October 2011
The flow rate can be increased by:
1. increasing the porosity of the filter, by increasing the quantity of burn-out material in the clay mix; and
2. increasing the pore size, either by
–
changing the particle size distribution of the burnout material, or by
–
changing the maximum firing temperature.
The bacteria removal effectiveness is only compromised when increasing the pore size